WhatsApp

water wastewater

Anionic vs Cationic Flocculants | Beta Pramesti Asia

BETAGARD anionic vs cationic flocculants for clarification, thickening, and dewatering, selected by solids, charge, shear, make-down, dose, and plant trials.

Anionic vs Cationic Flocculants | Beta Pramesti Asia

An anionic or cationic flocculant should be selected from the solids and water, not from a simple “opposite charge” rule. Operators should screen grades at bench scale, then prove make-down, dose, injection point, floc strength, overflow or filtrate quality, sludge or cake, consumption, and cost in a controlled plant trial.

PT Beta Pramesti Asia, through beta.co.id, supplies BETAGARD polymer flocculants for clarification, thickening, filtration aid, and dewatering in Indonesia. This page lists several anionic and cationic grades; the TDS, SDS, batch, and application test govern the final grade and use limits.

Technically reviewed: 31 July 2026.

When should an anionic or cationic flocculant be shortlisted?

Ionic charge helps form a shortlist, but performance also depends on charge density, molecular weight, product form, pH, salinity, temperature, solids type, coagulant, mixing energy, shear, and the separation unit. Compare candidates on the same sample and procedure.

Selection questionAnionic candidates are often screened whenCationic candidates are often screened whenDeciding evidence
What is the process duty?Mineral clarification, thickening, filtration aid, or solids responding to anionic bridgingOrganic-sludge conditioning or streams responding to cationic polymerBlank/control and a screen across charge densities
What are the solids?Mineral solids or surfaces showing a good test responseOrganic/biological sludge or surfaces showing a good test responseZeta/charge test where available, pH, TSS, volatile solids, oil, and floc observation
What constrains the unit?Shear, settling, recycle, filter, and carryoverShear, drainage, cake release, filtrate, and downstream effectTest at representative mixing, contact time, and equipment
What are the chemical risks?Overdose, residual polymer, slippery spills, lumps, and poor make-downThe same risks plus effects on biological or filtrate systemsDose sweep, SDS/TDS, compatibility, and acceptance criteria

This table is a screening framework, not a rule that one charge always fits one industry. The U.S. Bureau of Reclamation identifies polymer type, purpose, and testing as the basis for demand. The U.S. EPA dewatering manual also connects conditioning decisions to tests, equipment, handling, sludge volume, performance, and cost.

Which evidence is required before releasing a grade?

StageMinimum evidenceDecision
ProductName/grade, powder or emulsion form, charge, batch, TDS/SDS, shelf life, and package conditionMatch material to the approved trial
Make-downDilution water, concentration, wetting sequence, mixing energy, hydration/maturation time, solution age, and lumpsRelease, hold, or remake the solution
DosingPump output at backpressure, dose basis, flow/dry solids, injection point, dilution, interlock, and consumptionEstablish delivered rate, not just a setpoint
ResponseOverflow/filtrate, settling/drainage, floc size and strength, blanket, cake solids, capture, and downstream effectAccept a range, correct one variable, or reject
CommercialProduct use, make-down water, supporting chemicals, sludge, energy, downtime, and handlingCompare total cost per unit of water or solids

For cross-family screening, review industrial flocculants, PAC and ACH coagulants, and sludge-treatment programmes. Watermart dosing-pump capacity and materials should match the actual solution, pressure, and flow.

Flocculant-selection FAQs

Is a cationic flocculant always used for biological sludge?

Not always. It is a common screening point, not the final decision. Sludge source, surface charge, pH, salinity, oil, coagulant, shear, dewatering unit, filtrate, and downstream limits still have to be tested.

Is the highest-molecular-weight grade the most effective?

Not automatically. Molecular weight and charge density affect bridging, wetting, viscosity, shear sensitivity, and feed, but the result comes from the combination of product, make-down, mixing, injection point, solids, and equipment.

Which data should be sent for a shortlist?

Send water or sludge source, flow or dry-solids rate, pH, TSS and volatile solids, oil/organics, salinity, coagulant, separation unit, bench-test results, make-down, pump, overflow/filtrate/cake quality, and the operating problem through the PT Beta Pramesti Asia contact page.

Betagard Anionic and Cationic Oil Based Polymeric Flocculants

BETAGARD 6100

Anionic Flocculant

BETAGARD 6100 is an anionic polyelectrolyte, functioning as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is a highly charged anionic polymer, which will serve as an effective flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable for applications where the flocks formed are subject to high shear. Stock solutions are typically prepared at a concentration of 0.1 to 0.5%. Due to its low residual monomer content, BETAGARD 6100 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.

Technical Specifications

Physical FormBulk Density, gr/mlIonic ChargeMolecular WeightHandling and Storage MeasuresPackaging
Off white colored powder.0.65 - 0.90AnionicVery HighBETAGARD 6100 solution is essentially non-corrosive. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6100 should be stored in a dry place with an ambient temperature of not more than 38o C. Tightly close the drum container after use.Available in plastic container sizes of 15 kgs or PE bags up to 25 kgs.

Dosage & Usage Instructions:

The recommended dosage of BETAGARD 6100 for different applications is as follows:

  • Flocculant: 0.1 - 2.0 ppm
  • Coagulant Aid: 0.05 - 1.0 ppm
  • Filtration Aid: 0.01 - 1.0 ppm
  • Sludge Dewatering: 0.5 - 4.0 kg per ton of dry solids

The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for stirring. Such stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, further dilute the stock solution with clean water to 0.02% or less, prior to introduction to the process stream. However, this is usually determined by inspection of available facilities. Recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.

BETAGARD 6100 Series

RO & UF ANTISCALANT and WETTED SURFACE AIR COOLER SCALE INHOBITOR

Betagard 6100 Series is a multifunctional antiscalant and antifoulant for reverse osmosis systems, highly effective in controlling crystallization and particulate fouling on membrane surfaces.

Betagard 6100 will control the scale deposition of CaCO3, CaSO4, BaSO4, and CaF2. Betagard 6100 is formulated to control soluble and insoluble iron and actively disperse particulates. Effective against silica fouling, Hydro 600 is specifically designed for use on Thin Film and CA membranes.

Technical Specifications

Physical FormpHSp. Gravity at 25 DEG CHandling and Storage MeasuresPackaging
Colorless clear colored liquid.5.0 - 6.0AnionicKeep out of reach of children. In case of accidental splashing, flush with plenty of water. And for eye contact, must receive medical attention as a safety measure.Available in plastic container size with a net weight of 200 liters / drum.

Dosage & Usage Instructions:

Betagard 6100 is an aqueous solution of organic acids and is corrosive in concentrated form. Therefore, corrosion resistant dosing equipment should be used. Examples of suitable materials are 316L stainless steel or plastics such as GRP, PVC and PE. The recommended injection point is into the feed water downstream of filtration equipment and cartridge filters. Betagard 6100 is miscible with water in all proportions.

It can be applied as a neat product, or as a solution in distillate. A minimum dosage solution strength of 10% w/b is recommended. Betagard 6100 should be dosed continuously and in proportion to the feed water flow, to maintain the recommended dosing rate. The dosage rate required depends on the feed water quality and the saturation index of the various scale forming species present in the concentrated brine. The usual dosage rate range is between 5 - 15 ppm.

BETAGARD 6110

Anionic Flocculant

BETAGARD 6110 is an anionic polyelectrolyte, serving as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is a highly charged anionic polymer, which will serve as an effective flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable for applications where the flocks formed are subject to high shear. Stock solutions are typically prepared at concentrations of 0.1 to 0.5%. Due to its low residual monomer content, BETAGARD 6110 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.

Technical Specifications

Physical FormBulk Density, gr/mlIonic ChargeMolecular WeightHandling and Storage MeasuresPackaging
Off white colored powder.0.65 - 0.90AnionicVery HighBETAGARD 6110 solution is essentially non-corrosive. Recommended construction materials for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6110 should be stored in a dry place with an ambient temperature of no more than 38oC. Tightly close the drum container after use.Available in fiber drum or PE bag size - 25 kgs.

Dosage & Usage Instructions:

The recommended dosage of BETAGARD 6110 for different applications is as follows:

  • Flocculant: 0.1 - 2.0 ppm
  • Coagulant Aid: 0.05 - 1.0 ppm
  • Filtration Aid: 0.01 - 1.0 ppm
  • Sludge Dewatering: 0.5 - 4.0 kg per ton of dry solids

The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for stirring. Such stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, further dilute the stock solution with clean water to 0.02% or less, prior to introduction to the process stream. However, this is usually determined by inspection of available facilities. Recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.

BETAGARD 6120

Anionic Flocculant

BETAGARD 6120 is an anionic polyelectrolyte, serving as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is a highly charged anionic polymer, which will serve as an effective flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable for applications where the flocks formed are subject to high shear. Stock solutions are typically prepared at concentrations of 0.1 to 0.5%. Due to its low residual monomer content, BETAGARD 6120 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.

Technical Specifications

Physical FormBulk Density, gr/mlIonic ChargeMolecular WeightHandling and Storage MeasuresPackaging
Off white colored powder.0.65 - 0.90AnionicVery HighBETAGARD 6120 solutions are essentially non-corrosive. Recommended construction materials for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6120 should be stored in a dry place with an ambient temperature of no more than 38oC. Tightly close the drum container after use.Available in fiber drum or PE bag size - 25 kgs.

Dosage & Usage Instructions:

The recommended dosage of BETAGARD 6120 for different applications is as follows:

  • Flocculant: 0.1 - 2.0 ppm
  • Coagulant Aid: 0.05 - 1.0 ppm
  • Filtration Aid: 0.01 - 1.0 ppm
  • Sludge Dewatering: 0.5 - 4.0 kg per ton of dry solids

The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for stirring. Such stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, further dilute the stock solution with clean water to 0.02% or less, prior to introduction to the process stream. However, this is usually determined by inspection of available facilities. Recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.

BETAGARD 6130

Anionic Flocculant

BETAGARD 6130 is an anionic polyelectrolyte, serving as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is a highly charged anionic polymer, which will serve as an effective flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable for applications where the flocks formed are subject to high shear. Stock solutions are typically prepared at concentrations of 0.1 to 0.5%. Due to its low residual monomer content, BETAGARD 6130 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.

Technical Specifications

Physical FormBulk Density, gr/mlIonic ChargeMolecular WeightHandling and Storage MeasuresPackaging
Off white colored powder.0.65 - 0.90AnionicVery HighBETAGARD 6130 solutions are essentially non-corrosive. Recommended construction materials for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6130 should be stored in a dry place with an ambient temperature of not more than 38oC. Tightly close the drum container after use.Available in fiber drum or PE bag size - 25 kgs.

Dosage & Usage Instructions:

The recommended dosage of BETAGARD 6130 for different applications is as follows:

  • Flocculant: 0.1 - 2.0 ppm
  • Coagulant Aid: 0.05 - 1.0 ppm
  • Filtration Aid: 0.01 - 1.0 ppm
  • Sludge Dewatering: 0.5 - 4.0 kg per ton of dry solids

The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for stirring. Such stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, further dilute the stock solution with clean water to 0.02% or less, prior to introduction to the process stream. However, this is usually determined by inspection of available facilities. Recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.

BETAGARD 6140

Anionic Flocculant

BETAGARD 6140 is an anionic polyelectrolyte, serving as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is a highly charged anionic polymer, which will serve as an effective flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable for applications where the flocks formed are subject to high shear. Stock solutions are typically prepared at a concentration of 0.1 to 0.5%. Due to its low residual monomer content, BETAGARD 6140 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.

Technical Specifications

Physical FormBulk Density, gr/mlIonic ChargeMolecular WeightHandling and Storage MeasuresPackaging
Off white colored powder.0.65 - 0.90AnionicVery HighBETAGARD 6140 solutions are essentially non-corrosive. Recommended construction materials for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6140 should be stored in a dry place with an ambient temperature of not more than 38oC. Tightly close the drum container after use.Available in fiber drum or PE bag size - 25 kgs.

Dosage & Usage Instructions:

The recommended dosage of BETAGARD 6140 for different applications is as follows:

  • Flocculant: 0.1 - 2.0 ppm
  • Coagulant Aid: 0.05 - 1.0 ppm
  • Filtration Aid: 0.01 - 1.0 ppm
  • Sludge Dewatering: 0.5 - 4.0 kg per ton of dry solids

Actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for stirring. Such stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, further dilute the stock solution with clean water to 0.02% or less, prior to introduction to the process stream. However, this is usually determined by inspection of available facilities. Recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.

BETAGARD 6150

Anionic Flocculant

BETAGARD 6150 is an anionic polyelectrolyte, serving as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is a highly charged anionic polymer, which will serve as an effective flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable for applications where the flocks formed are subject to high shear. Stock solutions are typically prepared at a concentration of 0.1 to 0.5%. Due to its low residual monomer content, BETAGARD 6150 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.

Technical Specifications

Physical FormBulk Density, gr/mlIonic ChargeMolecular WeightHandling and Storage MeasuresPackaging
Off white colored powder.0.65 - 0.90AnionicVery HighBETAGARD 6150 solutions are essentially non-corrosive. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6150 should be stored in a dry place with an ambient temperature of no more than 38oC. Close the drum container tightly after use.Available in plastic drum size 15 kgs or PE bag - 25 kgs.

Dosage & Usage Instructions:

The recommended dosage of BETAGARD 6150 for different applications is as follows:

  • Flocculant: 0.2 - 2.0 ppm
  • Coagulant Aid: 0.1 - 1.0 ppm
  • Filtration Aid: 0.02 - 1.0 ppm
  • Sludge Dewatering: 0.5 - 4.0 kg per ton of dry solids

Actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for stirring. Such stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, further dilute the stock solution with clean water to 0.02% or less, prior to introduction to the process stream. However, this is usually determined by inspection of available facilities. Recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.

BETAGARD 6160

Anionic Flocculant

BETAGARD 6160 is an anionic polyelectrolyte, serving as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is a highly charged anionic polymer, which will serve as an effective flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable for applications where the flocks formed are subject to high shear. Stock solutions are typically prepared at a concentration of 0.1 to 0.5%. Due to its low residual monomer content, BETAGARD 6160 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.

Technical Specifications

Physical FormBulk Density, gr/mlIonic ChargeMolecular WeightHandling and Storage MeasuresPackaging
Off white colored powder.0.65 - 0.90AnionicVery HighBETAGARD 6160 solutions are essentially non-corrosive. Recommended construction materials for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6160 should be stored in a dry place with an ambient temperature of no more than 38oC. Close the drum container tightly after use.Available in plastic drum size 15 kgs or PE bag - 25 kgs.

Dosage & Usage Instructions:

The recommended dosage of BETAGARD 6160 for different applications is as follows:

  • Flocculant: 0.2 - 2.0 ppm
  • Coagulant Aid: 0.1 - 1.0 ppm
  • Filtration Aid: 0.02 - 1.0 ppm
  • Sludge Dewatering: 1.0 - 4.0 kg per ton of dry solids

Actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high-speed, high-shear mechanical mixers for stirring. Such stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, further dilute the stock solution with clean water to 0.02% or less, prior to introduction to the process stream. However, this is usually determined by inspection of available facilities. Recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.

BETAGARD 6170

Anionic Flocculant

BETAGARD 6170 is an anionic polyelectrolyte, serving as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is a highly charged anionic polymer, which will serve as an effective flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable for applications where the flocks formed are subject to high shear. Stock solutions are typically prepared at a concentration of 0.1 to 0.5%. Due to its low residual monomer content, BETAGARD 6170 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.

Technical Specifications

Physical FormBulk Density, gr/mlIonic ChargeMolecular WeightHandling and Storage MeasuresPackaging
Off white colored powder.0.65 - 0.90AnionicVery HighBETAGARD 6170 solution is essentially non-corrosive. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6170 should be stored in a dry place with an ambient temperature of no more than 38oC. Tightly close the drum container after use.Available in fiber drum or PE bag size - 15 kgs.

Dosage & Usage Instructions:

The recommended dosage of BETAGARD 6170 for different applications is as follows:

  • Flocculant: 0.2 - 2.0 ppm
  • Coagulant Aid: 0.1 - 1.0 ppm
  • Filtration Aid: 0.02 - 1.0 ppm
  • Sludge Dewatering: 1.0 - 4.0 kg per ton of dry solids

Actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high-speed, high-shear mechanical mixers for stirring. Such stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, further dilute the stock solution with clean water to 0.02% or less, prior to introduction to the process stream. However, this is usually determined by inspection of available facilities. Recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.

BETAGARD 6200

Cationic Flocculant

BETAGARD 6200 is a cationic polyelectrolyte, functioning as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is used primarily for wastewater purification, as well as for thickening and dewatering municipal and industrial sewage sludge (centrifuges, belt filter presses, chamber filter presses). This product is particularly suitable for applications where the formed flocks are subjected to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%.

Technical Specifications

Physical FormBulk Density, gr/mlIonic ChargeMolecular WeightHandling and Storage MeasuresPackaging
Off white colored powder.0.65 - 0.90CationicVery HighBETAGARD 6200 solution is essentially non-corrosive. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6200 should be stored in a dry place with an ambient temperature of not more than 38oC. Tightly close the drum container after use.Available in fiber drum or PE bag size - 15 kgs.

Dosage & Usage Instructions:

The recommended dosage of BETAGARD 6200 for different applications is as follows:

  • Clarification of secondary effluent: 1 - 5 ppm.
  • Flocculation, thickening, and dewatering of primary and secondary sludge of municipal sewage and of various industries: 0.5 - 4.0 kg per ton of dry solids.
  • Centrifugal operation: 1.5 - 5.0 kg per ton of dry solids.

The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for agitating. This stock solution is stable for at least two days without significant changes in its charge density that could affect its performance results. To ensure the stability of the solution, it is recommended to use water with a temperature lower than 40oC for dissolution, and the pH of the solution should be controlled within the range of 5.0 - 6.5. For best performance, before feeding to the process stream, further dilute the stock solution with clean water to 0.02% - 0.03% or less. Dilution can be done using in-line dilution or by using a dilution tank. However, this is usually determined by inspection of the facilities available. The recommended transfer pumps are gear type piston pumps or positive displacement piston pumps.

BETAGARD 6210

Cationic Flocculant

BETAGARD 6210 is a cationic polyelectrolyte, functioning as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is used primarily for wastewater purification, as well as for thickening and dewatering municipal and industrial sewage sludge (centrifuges, belt filter presses, chamber filter presses). This product is particularly suitable for applications where the formed flocks are subjected to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%.

Technical Specifications

Physical FormBulk Density, gr/mlIonic ChargeMolecular WeightHandling and Storage MeasuresPackaging
Off white colored powder.0.65 - 0.90CationicVery HighBETAGARD 6210 solution is essentially non-corrosive. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6210 should be stored in a dry place with ambient temperature not more than 38oC. Tightly close the drum container after use.Available in fiber drum or PE bag size - 25 kgs.

Dosage & Usage Instructions:

The recommended dosage of BETAGARD 6210 for different applications is as follows:

  • Clarification of secondary effluent: 1 - 5 ppm.
  • Flocculation, thickening, and dewatering of primary and secondary sludge of municipal sewage and of various industries: 0.5 - 4.0 kg per ton of dry solids.
  • Centrifugal operation: 1.5 - 5.0 kg per ton of dry solids.

The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for agitating. This stock solution is stable for at least two days without significant changes in its charge density that could affect its performance results. To ensure the stability of the solution, it is recommended to use water with a temperature lower than 40oCfor dissolution, and the pH of the solution should be controlled within the range of 5.0 - 6.5. For best performance, before feeding to the process stream, further dilute the stock solution with clean water to 0.02% - 0.03% or less. Dilution can be done using in-line dilution or by using a dilution tank. However, this is usually determined by inspection of the facilities available. The recommended transfer pumps are gear type piston pumps or positive displacement piston pumps.

BETAGARD 6220

Cationic Flocculant

BETAGARD 6220 is a cationic polyelectrolyte, functioning as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is used primarily for wastewater purification, as well as for thickening and dewatering municipal and industrial sewage sludge (centrifuges, belt filter presses, chamber filter presses). This product is particularly suitable for applications where the formed flocks are subjected to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%.

Technical Specifications

Physical FormBulk Density, gr/mlIonic ChargeMolecular WeightHandling and Storage MeasuresPackaging
Off white colored powder.0.65 - 0.90CationicVery HighBETAGARD 6220 solution is essentially non-corrosive. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6220 should be stored in a dry place with an ambient temperature of not more than 38oC. Tightly close the drum container after use.Available in fiber drum or PE bag size - 25 kgs.

Dosage & Usage Instructions:

The recommended dosage of BETAGARD 6220 for different applications is as follows:

  • Clarification of secondary effluent: 1 - 5 ppm.
  • Flocculation, thickening, and dewatering of primary and secondary sludge of municipal sewage and of various industries: 0.5 - 4.0 kg per ton of dry solids.
  • Centrifugal operation: 1.5 - 5.0 kg per ton of dry solids.

The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for stirring. This stock solution is stable for at least two days without significant changes in its charge density that could affect its performance results. To ensure the stability of the solution, it is recommended to use water with a temperature lower than 40oCfor dissolution, and the pH of the solution should be controlled within the range of 5.0 - 6.5. For best performance, before feeding to the process stream, further dilute the stock solution with clean water to 0.02% - 0.03% or less. Dilution can be done using in-line dilution or by using a dilution tank. However, this is usually determined by inspection of the facilities available. The recommended transfer pumps are gear type piston pumps or positive displacement piston pumps.

BETAGARD 6230

Cationic Flocculant

BETAGARD 6230 is a cationic polyelectrolyte, functioning as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is used primarily for wastewater purification, as well as for thickening and dewatering municipal and industrial sewage sludge (centrifuges, belt filter presses, chamber filter presses). This product is particularly suitable for applications where the formed flocks are subjected to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%.

Technical Specifications

Physical FormBulk Density, gr/mlIonic ChargeMolecular WeightHandling and Storage MeasuresPackaging
Off white colored powder.0.65 - 0.90CationicVery HighBETAGARD 6230 solution is essentially non-corrosive. Recommended construction materials for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6230 should be stored in a dry place with an ambient temperature of not more than 38oC. Tightly close the drum container after use.Available in fiber drum or PE bag size - 25 kgs.

Dosage & Usage Instructions:

The recommended dosage of BETAGARD 6230 for different applications is as follows:

  • Clarification of secondary effluent: 1 - 5 ppm.
  • Flocculation, thickening, and dewatering of primary and secondary sludge of municipal sewage and of various industries: 0.5 - 4.0 kg per ton of dry solids.
  • Centrifugal operation: 1.5 - 5.0 kg per ton of dry solids.

The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for agitating. This stock solution is stable for at least two days without significant changes in its charge density that could affect its performance results. To ensure the stability of the solution, it is recommended to use water with a temperature lower than 40oCfor dissolution, and the pH of the solution should be controlled within the range of 5.0 - 6.5. For best performance, before feeding to the process stream, further dilute the stock solution with clean water to 0.02% - 0.03% or less. Dilution can be done using in-line dilution or by using a dilution tank. However, this is usually determined by inspection of the facilities available. The recommended transfer pumps are gear type piston pumps or positive displacement piston pumps.

BETAGARD 6240

Cationic Flocculant

BETAGARD 6240 is a cationic polyelectrolyte, functioning as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is used primarily for wastewater purification, as well as for thickening and dewatering municipal and industrial sewage sludge (centrifuges, belt filter presses, chamber filter presses). This product is particularly suitable for applications where the formed flocks are subjected to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%.

Technical Specifications

Physical FormBulk Density, gr/mlIonic ChargeMolecular WeightHandling and Storage MeasuresPackaging
Off white colored powder.0.65 - 0.90CationicVery HighBETAGARD 6240 solution is essentially non-corrosive. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6240 should be stored in a dry place with an ambient temperature of not more than 38oC. Tightly close the drum container after use.Available in fiber drum or PE bag size - 25 kgs.

Dosage & Usage Instructions:

The recommended dosage of BETAGARD 6240 for different applications is as follows:

  • Clarification of secondary effluent: 1 - 5 ppm.
  • Flocculation, thickening, and dewatering of primary and secondary sludge of municipal sewage and of various industries: 0.5 - 4.0 kg per ton of dry solids.
  • Centrifugal operation: 1.5 - 5.0 kg per ton of dry solids.

The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for agitating. This stock solution is stable for at least two days without significant changes in its charge density that could affect its performance results. To ensure the stability of the solution, it is recommended to use water with a temperature lower than 40oCfor dissolution, and the pH of the solution should be controlled within the range of 5.0 - 6.5. For best performance, before feeding to the process stream, further dilute the stock solution with clean water to 0.02% - 0.03% or less. Dilution can be done using in-line dilution or by using a dilution tank. However, this is usually determined by inspection of the facilities available. The recommended transfer pumps are gear type piston pumps or positive displacement piston pumps.

Contact Us

Want to know more about BETAGARD Anionic and Cationic Oil Based Polymeric Flocculants? Contact us now to get more information or for technical consultation regarding the application of this product in your water treatment system.

Send Email to sales@beta.co.id