WhatsApp

mining

Aluminum Chlorohydrate

TERRAGARD EXSO 504 is a solvent-based cleaner formulated to remove oil, grease and other dirt from engines and parts.

Aluminum Chlorohydrate

PT Beta Pramesti Asia

TERRAGARD EXSO 504

Solvent Degreaser Cleaner

TERRAGARD EXSO 504 is a solvent-based cleaner formulated to remove oil, grease and other dirt from engines and parts. This product evaporates quickly, thus speeding drying without leaving a residue that can attract carbon dust, metal particles or other contaminants that can damage equipment.

Key Advantages

  • Efficiently removes oil, grease and dirt.
  • Vaporizes without leaving harmful residue.
  • Safe to use on a wide range of industrial equipment.
  • Suitable for general maintenance in manufacturing, automotive, marine and transportation industries.

Technical Specifications

PropertiesRated
AppearanceClear liquid
Sp. Gravity0.8-0.9
Water SolubilityInsoluble
Dosage & Instructions for UseUse directly on surfaces or parts that require cleaning, then dry.
Usage PrecautionsUse in a well-ventilated area and avoid contact with skin or eyes.
Packaging200L Drum or 20L Jerigen

How the Product Works

TERRAGARD EXSO 504 works through a rapid vaporization process that allows for deep cleaning without leaving a residue that could interfere with or damage equipment. Its chemical composition is designed to penetrate and dissolve oil and dirt without affecting the mechanical integrity of the engine or parts being cleaned.

Product Specifications

AppearanceOdorSpecific GravityFlash PointSolubility in WaterApplicationStoragePackaging
Clear colorless liquidSolvent0.75 - 0.85 g/cm³40°CInsolubleTERRAGARD EXSO 504 can be applied by immersion or soaking, using a brush or brush. For thick and hard oil or grease soiling, it is recommended to soak the equipment in TERRAGARD EXSO 504 for 5-10 minutes. Once the dirt is removed, wipe off and allow to dry.Do not store this product where the temperature is above 45°C or near strong oxidizing agents.Available in HDPE plastic 25 L/pail, 200 L/drum or 1000 L/IBC tank.

TERRAGARD EXSO 508

Solvent Degreaser for Industrial Maintenance

TERRAGARD EXSO 508 is a solvent-based cleaner formulated to remove oil, grease, and other dirt from machinery and parts. The product evaporates quickly, aiding the drying process without leaving a residue that can attract metal particles, carbon dust, or other contaminants that can damage equipment. It is suitable for general maintenance cleaning in the manufacturing, automotive, maritime and transportation industries.

Key Advantages

  • Removes oil and grease effectively.
  • Evaporates quickly without leaving residue.
  • Safe to use for a wide range of equipment.
  • Suitable for automotive, manufacturing and maritime industry maintenance.
  • Increases equipment longevity by preventing damage from particle contamination.

Technical Specifications

PropertiesDetails
AppearanceClear Liquid
Sp. Gravity0.79 - 0.81
Water SolubilityInsoluble
Dosage & Usage InstructionsApply directly on the contaminated area, leave for a few minutes, then wipe off with a cloth or brush.
Handling PrecautionsAvoid direct contact with skin and eyes, use in a well-ventilated area.
Packaging20L drum, 200L drum

How the Product Works

TERRAGARD EXSO 508 works through a rapid vaporization process, which enables the removal of residual oil, grease, and other dirt from metal surfaces without leaving traces or residue. With its solvent properties, it dissolves and removes contaminants, making cleaning and maintenance easier. Its special formula prevents the build-up of particles that can damage equipment in the long run.

Product Specifications

AppearanceOdorSpecific GravityFlash PointSolubility in WaterApplicationStoragePackaging
Clear colorless liquidSolvent0.75 - 0.85 g/cm³>77 °CInsolubleTERRAGARD EXSO 508 can be applied by immersion or soaking, using a brush or brush. For thick and hard oil or grease soiling, it is recommended to soak the equipment in TERRAGARD EXSO 508 for 5-10 minutes. Once the dirt is removed, wipe off and allow to dry.Do not store this product where the temperature is above 45°C or near strong oxidizing agents.Available in HDPE plastic 25 L/pail, 200 L/drum or 1000 L/IBC tank.

TERRAGARD GR 642

Water-based Cleaner

TERRAGARD GR 642 is an alkaline-based degreaser that acts as an all-purpose water-based cleaner and is specially formulated to remove oil, grease and dirt contamination from a variety of surfaces. This product is practical and easy to use by spraying, dipping, or brushing the metal surface to be cleaned with TERRAGARD GR 642.

Key Benefits

  • Effective in removing oil and dirt contamination from various types of surfaces.
  • Easy to use by spraying, dipping or brushing methods.
  • Safe to use as it is water-based and has low toxicity.
  • Suitable for various industrial metal cleaning applications.

Technical Specifications

PropertiesDetails
Flow RateN/A (Chemical Product)
Operating PressureN/A (Chemical Product)
Materials UsedHydrocarbon Solvent
Dimensions/Weight20L/200L drum
Installation RequirementsStore in a cool and well-ventilated place.
Maintenance SchedulePeriodically check the storage drum for leaks or damage.

How the Product Works

TERRAGARD GR 642 works by emulsifying oil and grease from contaminated surfaces. Once applied, it penetrates the dirt and breaks it down, allowing easy cleaning with water. With its slightly alkaline pH, it also helps protect metal surfaces from corrosion during the cleaning process.

Product Specifications

AppearanceSpecific GravitypHSolubility in WaterDosage & Feeding InstructionsHandling PrecautionsPackaging
Clear yellow liquid1.00 - 1.10 (at 20°C)8.5 - 9.5Completely soluble in waterThe application dosage of TERRAGARD GR 642 depends on the level of contamination and how heavy the dirt is. Dosage can typically range between 1:30 to 1:40 dilution.TERRAGARD GR 642 is alkaline and may cause irritation. Use eye protection and gloves when handling this product. In case of contact with eyes, rinse with water for 15 minutes and seek immediate medical attention.Packaged in 30 kg net weight plastic containers, 200 kg drums, or 1000 kg IBC tanks.

Contact Us

Interested in this product? Contact us now to get more information on how TERRAGARD Degreaser works and what it can do for your industry.

Contact Us