WhatsApp
By Marcus Somadjaja

A Small Dose, Big Power Savings: How Grinding Aids Cut Mill Energy

  • beta-pramesti-asia
  • industry-gold-dan-copper-mining
  • process-ore-crushing-grinding-dan

A Small Dose, Big Power Savings: How Grinding Aids Cut Mill Energy

Wet grinding can swallow 50–70% of a mine’s power, yet only ~1% fractures rock. A new push for chemical grinding aids and rheology modifiers aims to lower slurry viscosity by ~10%, raise solids loading, and unlock throughput gains that register in double digits.

Industry: Gold_&_Copper_Mining | Process: Ore_Crushing,_Grinding_&_Classification

Comminution (crushing plus grinding) is the energy sinkhole of mining. In typical operations, it takes the largest share of electrical power, with wet grinding alone often accounting for 50–70% of a plant’s total energy (www.mdpi.com). Only on the order of 1% of that input actually breaks mineral surfaces; most is lost to heat and noise (www.mdpi.com). As ore grades decline and finer grind sizes are required, any improvement in grinding efficiency—and water use—can move operating costs in a meaningful way (www.mdpi.com) (www.mdpi.com).

That’s why mines are testing specialty reagents—chemical grinding aids and rheology modifiers—to change how slurries flow. The thesis is simple physics: reduce slurry viscosity and yield stress (the stress needed to start flow), and the mill can run at higher % solids without choking, converting the same power into more tonnes ground.

Additives and slurry interaction mechanisms

Grinding aids and rheology modifiers are reagents that alter particle interactions in slurries (slurry rheology refers to the flow behavior of the mixture). By adsorbing on grain surfaces or altering the electrical double layer, they reduce particle–particle attraction and agglomeration. In practice these additives often contain functionalized polymers or surfactants—examples include glycols, amines, and anionic polymers—that “shield” mineral surfaces and introduce repulsive forces (www.mdpi.com) (www.mdpi.com).

Patents from Dow describe anionic polyacrylic polyelectrolytes that improve fragmentation at grain boundaries while cutting slime coating (www.mdpi.com). In effect, the additives keep fines dispersed instead of re-agglomerating and “lubricate” the granular slurry to lower its yield stress. Reviews summarize the outcome: well-chosen chemical additives “promote grinding efficiency, decrease water consumption, improve material mobility, and narrow the particle size distribution of the grinding products” (www.mdpi.com). Vendors of specialty reagents for circuits in gold and copper concentrators, such as those under /products/mining, position these polymeric dispersants specifically for this role.

First principles and experiments show that adding an effective aid at low dosages can reduce low-shear viscosity or yield stress by on the order of 10% or more (rheology measured, for example, by a Brookfield viscometer at 25°C and 5 rpm) (patents.google.com) (patents.google.com). Typical plant-relevant dosing is a few tens of grams per tonne of ore—e.g., 30–100 g/t (≈0.003–0.01% w/w)—for a polymeric dispersant to deliver ~10% viscosity reduction (patents.google.com) (patents.google.com).

Solids loading and mill performance

Slurry rheology (especially yield stress and low-shear viscosity) is strongly correlated with mill power draw, particle breakage rates, and fines production; lowering yield stress with additives directly boosts grinding uniformity (www.mdpi.com). With additives, the mill can operate at higher % solids in the charge. Dow’s work suggests optimum grinding occurs at ~70–88% solids (w/w) (patents.google.com), whereas untreated slurry would demand lower density to avoid jamming (e.g., 60–65%). At equal water flow one can increase the ore load by 10–20 percentage points.

Raising solids content reduces the volume of water to be pumped and heated. In a ball mill circuit, each pass handles more ore per unit energy. Many companies observe that, for fixed mill power, throughput rises nearly in proportion to solids fraction. Gains of tens of percent have been reported. A lab study on magnetite found that a polysaccharide-based grinding aid (Zalta VM1122) cut specific energy from 18.0 to 12.4 kWh/t—a 31.1% reduction—while achieving a finer product (P80 from 181 to 142 µm; P80 is the 80th-percentile particle size) (ltu.diva-portal.org). Analogous improvements are documented in cement grinding: one industry report found all tested additives delivered significant energy savings versus baseline (www.mdpi.com). Typical improvements in case studies range from ~5% for marginal cases up to 30–50% in optimized conditions (www.mdpi.com) (ltu.diva-portal.org). Patents also note that such anionic polymers, at modest doses, do not detrimentally affect downstream processes—e.g., flotation recoveries for copper, zinc, and gold (patents.google.com).

Quantitative trial metrics and targets

  • Viscosity reduction: lab rheometer tests quantify how a candidate additive lowers viscosity at representative shear. Routine Brookfield or rheometer measurements (e.g., 25°C, 5 rpm spindle) are standard. A practical target is at least a ~10% viscosity drop at optimal dose (patents.google.com).
  • Throughput increase: at constant mill power or filling, higher pulp density typically yields more throughput, often ~10–20% higher solids retention for a given pump flow. Compare mass of ore ground per hour vs. baseline. Case studies suggest up to ~30% increase is possible (ltu.diva-portal.org).
  • Energy savings: record specific energy (kWh/t) and mill power. Effective additives should lower kWh/t; reductions of 10–30% have been documented (www.mdpi.com) (ltu.diva-portal.org). Even a 5% saving can translate to large absolute kWh/year at scale.
  • Grinding fineness: monitor product size (P80). In the magnetite test, P80 fell by ~20% with additive (ltu.diva-portal.org).
  • Downstream performance: check flotation recovery and water clarity. Patents report that well-chosen anionic polymers “usually do not detrimentally affect” flotation of copper, zinc, gold, etc. (patents.google.com). Also monitor any change in froth lifetime.

Plant trial methodology

Baseline characterization involves logging current operating points before any additive: mill feed rate, slurry solids %, power draw, product particle size distribution (PSD), and flotation recovery. Slurry viscosity or yield stress serves as the control, measured with a field viscometer or portable rheometer.

Pilot or batch screening can be run with site ore in a lab or pilot mill. Slurries at target pulp densities receive graded doses (e.g., 0, 25, 50, 100 g/t). Viscosity versus shear is measured to select a dose that gives a meaningful drop (often around the point of diminishing returns), noting that small doses (≪1%) are typical and many effective doses are in the 0.005–0.01% range by weight (patents.google.com). A control slurry without additives will show rising viscosity as solids are loaded.

Incremental addition on the full-scale mill starts at the nominal dosing point (for example, just before the ball mill feed or in the cyclone feed box). Stepwise increases are made during stable operating intervals while monitoring power, load, slurry density, and flow. An accurate chemical metering setup—such as a dedicated skid using an inline dosing pump—keeps addition consistent with the chosen grams-per-tonne target. Simultaneously, periodic samples are taken for PSD analysis.

Performance monitoring for each run (with and without additive) captures throughput (t/h), net grinding energy (kWh/t), and product size. Downstream checks include flotation recovery and concentrate grade to confirm metallurgical stability. Measuring slurry friction in pipelines or across pumps adds insight; a lower pump head at fixed flow indicates reduced viscosity. A good sign is reduced pump energy or improved slurry flow for the same pump speed.

Data analysis comprises percentage gains versus baseline—for example, “with 50 g/t additive, mill throughput rose by X% while power draw was Y% lower”—and plots of efficiency metrics (energy vs. solids) for each dosage to confirm that increased solids % or feed rate tracks lower torque at constant feed.

Economic assessment compares chemical cost to energy savings or extra production. Even a small kWh/t reduction can justify a reagent if gains are stable. Accounting for consumables is part of the check; no increase in ball wear or liner wear was found in trials (www.mdpi.com).

Optimization and scale-up typically locate a dosage optimum beyond which benefits plateau (www.researchgate.net). Integration into normal operation follows if results are positive, with ongoing monitoring because ore variability alters rheology; dose is adjusted using online viscosity meters or process feedback.

Bottom-line efficiency gains

Careful selection and testing of grinding aids and rheology modifiers let mills run at higher pulp densities with lower viscosity. In practice, modern additives—typically polymeric or surfactant-based—can lower low‑shear viscosity by ~10% with only a few grams per tonne (patents.google.com) (patents.google.com). Campaign trials have enabled up to tens of percent increase in production—or equivalent power reduction—in comminution (ltu.diva-portal.org) (www.mdpi.com). Metallurgists proving the business case rely on rigorous A/B data collection under otherwise identical conditions and on fit-for-purpose mining reagents, such as those in /products/mining, matched to their ore and water chemistry.

Sources: Authoritative studies and industry reports on comminution and grinding aids (www.mdpi.com) (www.mdpi.com) (www.mdpi.com) (patents.google.com) (patents.google.com) (patents.google.com) (patents.google.com) (ltu.diva-portal.org). All data trends and figures above are sourced from these peer-reviewed articles, patents, and technical reviews.