WhatsApp
By Marcus Somadjaja

The Mining Water Squeeze: How Smarter Thickeners and Flocculants Are Rewiring Grinding Circuits

  • beta-pramesti-asia
  • industry-gold-dan-copper-mining
  • process-crushing-and-grinding

The Mining Water Squeeze: How Smarter Thickeners and Flocculants Are Rewiring Grinding Circuits

Gold and copper mills are closing the loop on water. The combination of high‑performance tailings thickeners and tuned flocculant chemistry is pushing reuse above 90% and slashing fresh draw.

Industry: Gold_&_Copper_Mining | Process: Crushing_and_Grinding

Crushers and mills in gold/copper plants consume vast quantities of water — often several thousand liters per tonne of ore (smartwatermagazine.com). Digital plant modeling is changing that equation: real‑time monitoring can cut usage from about 4,000 L/t to under 1,000 L/t (smartwatermagazine.com).

Across the industry, the priority is simple: recycle thickener overflow and filtered water back to the mills, swap in alternative sources such as seawater where feasible, and optimize comminution for water efficiency (mdpi.com; ceecthefuture.org). Ambitions are rising: sector targets call for ~50% cuts over a decade (Canada’s CMIC goal) and majors such as Anglo American aim for ~30% freshwater reduction by 2030 (ceecthefuture.org).

In practice, mines in arid belts have already shifted entirely to seawater for crushing and grinding — reserving scarce fresh water for flotation (ceecthefuture.org). High‑density comminution units, like HPGRs (high‑pressure grinding rolls) or stirred mills, run with lower slurry volumes than conventional SAG (semi‑autogenous) and ball circuits, cutting both energy and water; replacing SAG–Ball with HPGR–Vertimills can reduce comminution energy roughly 40% while also lowering circuit water (ceecthefuture.org).

Closed‑loop water accounting

Digitally enabled water accounting — pH/salinity monitoring and modeling — allows mills to reuse more water without process upsets (smartwatermagazine.com; mdpi.com). Simulators now factor dissolved‑ion build‑up in recycled streams so operators only flush or treat rejects when needed (smartwatermagazine.com; mdpi.com).

The end‑state is a closed‑circuit water strategy: recover more than 80–90% of process water via recycle — now standard to meet regulations and costs (mdpi.com; ceecthefuture.org).

Recycling streams into the mill

Tailings‑tank overflows and filtrate streams are routed back to grinding; simulation work suggests 88–95% of tailings water can be reused if thickeners and filters are optimally applied (mclanahan.com; processingmagazine.com). In practice, primary thickeners recover about 90% of slurry water by volume, and with secondary thickening this can exceed 95% (processingmagazine.com; processingmagazine.com).

Where available, seawater or treated effluent displaces freshwater in the grinding circuit; several large Chilean copper mines already run crushers and mills on desalinated seawater (mdpi.com; ceecthefuture.org).

Tailings thickener performance and clarity

Tailings thickeners separate slurry into a dense underflow and a clarified overflow (underflow = concentrated solids, overflow = clear liquor). The overflow is typically returned to the grinding/flotation circuit. Modern “high‑rate” and deep‑cone designs achieve very low moisture tailings: FLS Deep Cone thickeners can reach at least 70% solids in underflow (fls.com). Thickeners also operate as clarifiers — a role analogous to a clarifier used to remove suspended solids — and a well‑run unit can recover on the order of 90% or more of tailings water (processingmagazine.com).

Case studies quantify the lift. At a large iron‑ore concentrator, a high‑rate thickener (35% solids underflow) produced an overflow of 1,588 m³/h (cubic meters per hour), equivalent to more than 88% of tailings water available for reuse (mclanahan.com). At South Africa’s Khumani iron‑ore mine, two‑stage thickening — high‑rate, then paste — reclaimed roughly 90% of slurry water by volume in the first stage and an additional 75–80% in the second, yielding more than 95% total recovery (processingmagazine.com; processingmagazine.com).

In general, paste‑thickened tailings (90–85% solids) release almost no free water at the plant site — a South African platinum study found “significant water savings” only when tailings were thick enough to have almost no free water (scielo.org.za). Denser tailings (60–75% solids) likewise shrink dam footprints and capture far more water for recycle (fls.com; processingmagazine.com).

Overflow quality (turbidity/clarity) determines whether water flows straight back to grinding. Clear overflow allows direct reuse; if not, further treatment (for example, filtration) may be needed. Properly flocculated thickeners often produce overflow simple enough for reuse, avoiding fresh make‑up water.

Flocculants and settling control

Chemical flocculants — typically high‑molecular‑weight polyacrylamides or co‑polymers — aggregate fines into larger flocs, boosting settling rates, underflow density, and overflow clarity. Plants deploy targeted flocculants to accelerate tailings settling and clean up thickener overflow for recycle.

Quantified gains are material. A large‑scale concentrator study showed that increasing flocculant dose and raising slurry pH increased thickener underflow solids and sharply improved overflow clarity (researchgate.net). The same optimization — floc dosing of about 8–13 g/t (grams per tonne) and pH raised from roughly 8 to 11 — cut net water consumption by 23%, translating to $576,000 in annual savings (researchgate.net).

Flocculant chemistry has also lifted throughput. CSIRO reports “synthetic flocculants enable much larger aggregates…leading to much higher mass throughputs and greatly reduced thickener diameter” (research.csiro.au). Cleaner overflow reduces — or eliminates — the need for downstream water treatment; with lower turbidity, mills can recycle clarified water without adding coagulants or extra filters.

Dosing, monitoring, and setpoints

Effective flocculation depends on control of dosage, dilution, and feed conditions. Industry practice shows benefits from spreading polymer injection along the feedwell and operating slightly alkaline to maximize performance (researchgate.net). On‑line controls — rake torque and overflow turbidity meters — are used to adjust polymer feed and underflow pump speed in real time (fls.com). Typical flocculant ranges of 1–20 g/t are reported in modern operations, with exact setpoints tailored to slurry characteristics.

Accuracy matters at low doses, which is why mills pair polymer trains with an exacting dosing pump to keep addition rates on target and overflow clarity stable.

Compliance and sustainability settings

Recovering and reusing thickener overflow is often required in water‑scarce jurisdictions. Regulations in water‑stressed regions such as Peru, Chile, and Australia drive high recycling rates. Indonesian mining guidelines emphasize minimizing effluent discharge; while no specific “water reuse” quota is set, companies implement thickening to meet environmental licenses. In practice, proper thickening and flocculant use allow gold/copper operations to approach near‑zero freshwater addition and meet stringent turbidity/emissions standards.

Bottom line on grinding‑circuit water

A well‑designed thickening train — often two‑stage, high‑rate plus paste — plus optimized flocculant dosing typically delivers 90–95%+ water reuse, sharply trimming raw‑water cost and tailings footprint (processingmagazine.com; processingmagazine.com). The economic gains (lower water bills, higher throughput, “dry” tailings) and environmental benefits (less freshwater withdrawal, safer tailings dams) are significant, which is why thickener/flocculant optimization has become a priority across gold/copper operations (researchgate.net; processingmagazine.com).

Citations: Latest industry and technical literature on comminution water use (smartwatermagazine.com; mdpi.com; ceecthefuture.org), thickener performance (mclanahan.com; processingmagazine.com; processingmagazine.com), and flocculation studies (researchgate.net; research.csiro.au). (See references for full source metadata.)